TXIB

Stay updated with Bastone Plastics' news and insights. Explore daily plasticizer price updates, expert blogs on PVC resin and plasticizer applications, product comparisons, and coverage of events and exhibitions we attend worldwide.

bastone blog page banner

Tag TXIB

TXIB vs DINP

image 11

DINP is a general-purpose phthalate plasticizer that can make up the whole plasticizer loading of a flexible formulation, and TXIB is a low-viscosity non-phthalate additive that replaces a few phr of the primary plasticizer to thin a plastisol. In the…

What is Plasticizer TXIB(STONE TXIB)

Stone TXIB is an excellent analogue/substibution of EASTMAN TXIB

Brief introduction TXIB plasticizer is recognized as an advanced primary plasticizing agent for PVC plastisol systems. This high-performance formulation demonstrates exceptional compatibility with polyvinyl chloride resins and polyurethane-based materials, while maintaining effective interaction with conventional primary and secondary plasticizers. The…