Factory and Activities
Product datasheet
Specifications
Isononyl alcohol — clear liquid, Bastone production grade.
| Product name | Isononyl alcohol (INA) |
| Manufacturer | Bastone Plasticizer |
| Batch no. | BST1565141 |
| Storage tank no. | 2G-915 |
| Sampling date | 2026-05-14 |
| Execution standard | Internal contract technical requirement 2026-037 |
| Property | Specification | Test result | Test method |
|---|---|---|---|
| Purity, % (mass fraction) | ≥ 99.0 | 99.700 | GZHLH-T4.719.23.301.2026 |
| Color, Pt-Co | ≤ 10 | 3 | GB/T 6324.6-2014 |
| Water content, % (mass fraction) | ≤ 0.1 | 0.013 | GB/T 6283-2008 |
| Acid value, mgKOH/g | ≤ 0.1 | 0.042 | GZHLH-T4.719.23.342.2026 |
End-use
Applications
INA esterifies with phthalic anhydride to produce DINP, the leading replacement plasticizer for DEHP in flexible PVC cable, flooring, and film. The branched C9 structure gives finished plasticizer better low-temperature flexibility and migration resistance than straight-chain alcohol esters.
The same feedstock also supports synthesis of DINA-series adipate plasticizers and isononyl-ester lubricant base stocks, where low acid value and tight color specification reduce downstream catalyst deactivation and finished-product color drift.
DINP esterification
Reacted with phthalic anhydride for flexible PVC cable, flooring, and film compounds.
DINA synthesis
Adipate ester route for low-temperature flexible PVC and gasket compounds.
Ester-based lubricants
Feedstock for synthetic ester base oils where color stability matters.
Procurement
Why Source Through Bastone Plasticizer
Bastone operates its own isononyl alcohol production line, giving buyers confirmed allocation directly from the manufacturer rather than spot-market resale. Every shipment carries a batch-traceable quality certificate against contract spec 2026-037, verifiable at goods receipt without relying solely on incoming QC.
- In-house production — confirmed supply directly from Bastone's own manufacturing line, with full scheduling visibility.
- Batch-traceable COA — every shipment ships with documentation matched to the originating production batch.
- Technical support — grade selection and esterification process input for buyers comparing C9 alcohol feedstocks.
- Export documentation — COA, MSDS, and customs paperwork handled directly, without third-party trading delays.
Trade terms
Sourcing and Logistics
| Supply origin | Bastone Plasticizer production facility, Ningbo, China |
| Packaging | 200L steel drums; ISO tank, bulk |
| Documentation | COA, MSDS, packing list, commercial invoice, bill of lading |
| Trade terms | FOB Ningbo / Shanghai; CIF negotiable |