TCEP Tris(2-Chloroethyl) Phosphate — Flame Retardant Plasticizer (CAS 115-96-8)

Bastone supplies TCEP (Tris(2-chloroethyl) phosphate, CAS 115-96-8) as a halogenated organophosphate flame retardant plasticizer for PVC, polyurethane, phenolic resins, and cellulose-based polymers. With combined chlorine and phosphorus content delivering dual-mechanism flame suppression, TCEP serves demanding applications where standard plasticizers cannot meet fire safety requirements.

Molecular Formula: C6H12Cl3O4P8

Other Synonyms: Tri(beta-chloroethyl) phosphate

Packaging: 200L drum; IBC

Description

TCEP is a chlorinated organophosphate ester produced by the reaction of phosphorus oxychloride with ethylene oxide. The structure contains three 2-chloroethyl groups bonded through phosphate linkages, yielding a molecule with 10.5–10.8% phosphorus and 37.0–37.3% chlorine by weight. Both elements contribute to flame retardancy through separate but complementary pathways — the phosphorus disrupts combustion chemistry in the condensed phase, while the chlorine generates halogen radicals that interrupt the gas-phase flame chain reaction.

The physical properties of TCEP make it easy to work with in standard compounding equipment. Viscosity at 25°C falls between 38 and 42 mPa·s — low enough for efficient incorporation into PVC plastisols or polyurethane systems without extended mix times or elevated processing temperatures. Density at 20°C runs from 1.410 to 1.430 g/cm³, which formulators need to account for when converting weight-based formulations to volume-based production batches. Acid value is held to ≤0.1 mgKOH/g, keeping the compound from accelerating degradation in pH-sensitive polymer systems.

The flash point of ≥220°C gives TCEP a safe handling and processing window that aligns with typical PVC processing temperatures. Color is controlled to ≤50 on the Platinum-Cobalt scale, producing a material that will not introduce visible discoloration into light-colored or transparent formulations. Water content is capped at ≤0.10%, which matters in moisture-sensitive systems such as polyurethane foams, where residual water triggers unwanted blowing or chain-extension side reactions.

TCEP functions primarily as a flame retardant additive, but the datasheet also positions it as a co-plasticizer — used alongside primary plasticizers like DOP or DINP to extend flame retardant effect without sacrificing flexibility. At Bastone, we produce TCEP alongside our core plasticizer portfolio, which means technical staff can advise on complete formulation packages rather than treating TCEP as a standalone procurement item.

Factory and Activities

TCEP Tris(2-Chloroethyl) Phosphate — Flame Retardant Plasticizer (CAS 115-96-8) - BASTONE Plastics

Specifications

TCEP supplied as a clear to pale yellow liquid
TCEP supplied as a clear to pale yellow liquid, ready for direct incorporation into polymer systems.

General Information

Property Detail
Product Name Tris(2-chloroethyl) phosphate
Abbreviation TCEP
CAS Number 115-96-8
Chemical Type Halogenated organophosphate ester
Molecular Formula C₆H₁₂Cl₃O₄P
Appearance Clear to pale yellow liquid
Export Entity Zhejiang Bastone Technology Co., Ltd

Technical Properties

Parameter Specification Unit
Acid Value ≤0.1 mgKOH/g
Chroma (Platinum-Cobalt) ≤50 —
Viscosity (25°C) 38–42 mPa·s
Density (20°C) 1.410–1.430 g/cm³
Refractive Index (nD25) 1.470–1.479 —
Flash Point ≥220 °C
Phosphorus Content 10.5–10.8 %
Chlorine Content 37.0–37.3 %
Water Content ≤0.10 %

Applications

TCEP as a flame retardant plasticizer in PVC cable jacketing
TCEP as a flame retardant plasticizer in PVC cable jacketing and flexible polymer extrusion lines.

Flexible PVC and PVC compounds represent the largest use for TCEP. Cable jacketing, upholstery coatings, and protective sheeting that must pass vertical flame tests benefit from the dual phosphorus-chlorine mechanism. In practice, TCEP is rarely used as the sole plasticizer — it is blended with a primary plasticizer (DOP, DINP, or DOTP) to achieve the target LOI or UL94 rating without reducing flexibility below specification.

Polyurethane foams — both rigid and flexible — use TCEP to meet fire standards in furniture, mattress covers, and automotive interior panels. In flexible polyurethane systems, TCEP's low viscosity allows incorporation as a liquid additive during the polyol premix stage. The low water content (≤0.10%) is essential here; excess moisture in a polyurethane system will react with isocyanate groups and generate CO₂, creating unwanted voids or altering the density profile of the finished foam.

Cellulose acetate and cellulose nitrate films and coatings have historically relied on chlorinated phosphate esters as both plasticizers and flame suppressants. Cellulose nitrate in particular is highly flammable and requires co-additives with high active halogen content; TCEP's 37% chlorine concentration addresses that requirement while contributing to film flexibility.

Phenolic and epoxy resins used in laminated boards, printed circuit boards, and industrial coatings incorporate TCEP where flame retardancy is a regulatory or end-use requirement. At processing temperatures common for these thermosets, TCEP's flash point of ≥220°C provides an adequate safety margin during mixing and casting.

Polyimide processing and specialty lubricant or fuel additive applications are listed in the product datasheet as additional uses, reflecting the chemical stability of the phosphate ester backbone under thermal stress. Metal extractants in hydrometallurgical processes also utilize organophosphate compounds in their formulation chemistry.

Why Source Through Bastone

TCEP available in IBC containers and steel drums
TCEP available in IBC containers and steel drums for bulk export and industrial supply chain delivery.

Bastone operates four production sites and a dedicated R&D center in the Hangzhou Economic Development Zone. Quality consistency comes from in-house manufacturing — incoming raw material specs, intermediate process controls, and final product release testing all run through the same technical team. Batch records and COAs ship with every order, and our technical service group can provide SDS documentation, regulatory compliance letters, and formulation guidance as part of the standard commercial relationship.

For buyers sourcing TCEP as part of a broader plasticizer or additive program, Bastone's full product range — DOP, DOTP, DINP, DOA, TOTM, and specialty additives — means consolidating purchases with a single qualified supplier. Consolidated orders reduce logistics complexity, streamline supplier audit workloads, and give buyers more leverage on pricing and scheduling.

On the compliance side, Bastone's export team handles documentation for major trade lanes regularly and can prepare REACH compliance statements, MSDS packs for target markets, and country-of-origin documentation needed for customs clearance.

Sourcing & Logistics

Item Detail
Packaging 250 kg iron drums; 1,250 kg IBC
Export Entity Zhejiang Bastone Technology Co., Ltd
Port of Loading Ningbo / Shanghai
Trade Terms FOB, CIF, CFR (negotiable)
Documentation COA, SDS, packing list, commercial invoice, B/L
Sample Availability Available on request
Minimum Order Contact sales for MOQ by market

Contact Bastone at [email protected] for pricing, lead times, and technical data packages.

TEP Triethyl Phosphate (CAS 78-40-0) — Flame Retardant Plasticizer for PVC and CoatingsTEP Triethyl Phosphate (CAS 78-40-0) — Flame Retardant Plasticizer for PVC and Coatings
Bastone's TEP (triethyl phosphate) is a high-purity organophosphate…
TCPP (Tris(1-Chloro-2-Propyl) Phosphate) | Flame Retardant Plasticizer — CAS 13674-84-5TCPP (Tris(1-Chloro-2-Propyl) Phosphate) | Flame Retardant Plasticizer — CAS 13674-84-5
Bastone STONEAF-TCPP is a chlorinated organophosphate flame retardant…
TXP Trixylenyl Phosphate — Flame-Retardant Plasticizer & Lubricant Additive (CAS 25155-23-1)TXP Trixylenyl Phosphate — Flame-Retardant Plasticizer & Lubricant Additive (CAS 25155-23-1)
Trixylenyl phosphate (TXP) is an organophosphate ester produced…

Online Message

If you have any questions, you can leave a message here, we will contact you within 24 hours

Contact us

Get quote for your products or ask for a unique solution . We are here to provide quality products and flexible service.