Brief Introdcution
Plasticizer DINP(Diisononyl Phthalate, CAS 28553-12-0/68515-48-0), is a phthalate PVC plasticizer used to make PVC more flexible
Chemical structure:

Technical date sheet of DINP
| Items | Specification |
|---|---|
| Appearance | Transparent oily liquid without suspended matter |
| Purity, wt% | ≥99.5 |
| Chroma, (Platinum-Cobalt) No. | ≤30 |
| Acid Value, mgKOH/g | ≤0.06 |
| Density, g/cm3 | 0.968-0.978 |
| Volume resistivity, ×109Ω·m. | ≥2.0 |
| Moisture, % | ≤0.10 |
| Flash point, ℃ | ≥214 |
Appplication of Plasticizer DINP
DINP is ideal for long-life, flexible PVC applications. It is widely used in the following industries:
- Flexible PVC products
Electrical cables and wires
- Vinyl flooring
- PVC leather and coated fabrics
- Automotive interiors
- Wall paper
- Building and construction materials(Membrance)
- Sealants and adhesives
- Hoses and tubing
Is DINP Safe?
DINP has been extensively studied for health and environmental impacts. Accordingly, DINP is authorized for use in many industrial applications
However, regulations in some regions restrict its use in:
- Toys that can be placed in the mouth
- Food contact materials
Therefore, for sensitive applications, non-phthalate alternatives such as DOTP or DOA are often recommended.
At BASTONE, we supply high-quality plasticizers including DINP, DOP, DOTP, DOA, and DPHP. Explore our plasticizers or contact us to learn more.
Additonal information
TOP Plasticizer DINP suppliers in the market
BASF SE Polynt SpA Exxon Mobil Corporation LG Chem Ltd Nan Ya Plastics Corporation Zhejiang Bastone Technology Co.,Ltd