Dioctyl Terephthalate (DOTP) is an environmentally friendly plasticizer usded in PVC. One of the main industrial methods to synthesize DOTP is the direct esterification method, also known as the TPA method, which uses terephthalic acid (TPA) and 2-ethylhexanol as raw materials. BASTONE is the leading DOTP manufacturer and supplier in China, with years of experience as a reliable producer and exporter of plasticizers.

1. Chemical Reaction

The core chemical reaction for producing DOTP via the TPA method is as follows:

Chemical reaction for producing DOTP, Bastone the leading DOTP Manufactuer in China

Under the action of a catalyst and elevated temperatures, terephthalic acid reacts with 2-ethylhexanol to form DOTP and water. The reaction proceeds until the acid value of the mixture drops below 0.2 mg KOH/g, indicating the completion of esterification.

2. Process Flow

The production of DOTP by the direct esterification method involves several stages:

  1. Raw Materials Preparation
    Mix Terephthalic acid (TPA) and 2-ethylhexanol (2-EH) in a reactor along with a suitable catalyst.
  2. Esterification Reaction
    The mixture is heated under atmospheric pressure. Water formed during the reaction is continuously removed to drive the reaction to completion. Heat transfer oil is used to maintain the required temperature.
  3. Neutralization
    Neutralized to remove residual acidity.
  4. Dehydration and De-alcoholization
    Remove residual water and unreacted alcohol from the product.
  5. Water Washing and Filtration
    The product is washed with water to remove impurities and neutral salts, then filtered to remove any suspended solids.
  6. Final Product Isolation
    Get final DOTP after Isolation.
DOTP Production Process DOTP Manufacturer

3. Equipment Layout

image 2
  • A reactor vessel for esterification, fed with PTA (TPA) and 2-EH.
  • A reflux and condensation system for recovering unreacted alcohol.
  • A heat exchanger to control temperature.
  • A vacuum line and vent for removing water and gases.
  • Neutralization and separation units for purification.
  • Filtration system to finalize product quality.

4. Advantages of the TPA Method

  • Low production cost
    PTA is cheaper than traditional phthalic anhydride.
  • Better product performance
    DOTP made via this route has low volatility, excellent electrical insulation, and environmental safety.
  • Cleaner process
    Minimal by-products and better environmental compliance.

BASTONE Plasticizers Enhance the performance of your PVC products. Find costing-saving plasticizer DINP, DOTP, DOP, DOP, DPHP, DBP, DIBP at our site https://bastoneplasti.wpenginepowered.com

BASTONE is the leading DOTP Producer in china. DOTP is a premium plasticizer.

Newsletter Updates

Enter your email address below and subscribe to our newsletter