Category Blogs

Sharing the latest advancements of product insights, market trends, technological innovations​​ including plasticizer and PVC formulation, production process etc

Wear-Resistant PVC Leather Production Process Study

PVC Leather

PVC artificial leather, also known as polyvinyl chloride (PVC) synthetic leather, is produced by mixing PVC resin with additives such as plasticizers, stabilizers, fillers, and pigments. These components are then processed through coating, embossing, and printing techniques. PVC artificial leather…

 Plasticizer DOTP in PVC artificial leather Production

Plasticizer DOTP

Plasticizer DOTP​​ (dioctyl terephthalate) has emerged as a cornerstone for manufacturing high-performance PVC synthetic leather. Renowned for its exceptional plasticizing efficiency and thermal stability, DOTP plays a pivotal role in transforming rigid PVC into soft, flexible, and durable materials used…