Plasticizers for PVC Flooring
Vinyl flooring has to pass indoor-air emission tests, lie flat for decades, resist stains in the wear layer, and coat cleanly at line speed. The plasticizer package controls every one of those outcomes.
Plasticizer Selection Across Every Flooring Layer
Modern vinyl flooring is a stack of layers: a clear wear layer, a printed decor film, a compact or foamed core, and a backing. Each layer carries its own plasticizer level, from roughly 20–35 phr in a highly filled LVT core to 50 phr or more in a cushioned foam layer.
Choosing plasticizers for PVC flooring sets emission levels, dimensional stability, stain resistance, and plastisol viscosity all at once. Our article on plasticizers for PVC flooring compliance and performance covers the regulatory side in depth.
Bastone supplies four core grades for flooring producers: DOTP for LVT and commercial sheet, DINCH for ultra-low-emission residential and school floors, DINP for high-wear industrial goods, and TXIB as a viscosity reducer and stain-resistance aid in wear layers.
Key Performance Challenges in Vinyl Flooring
Flooring failures rarely show up at the plant. They appear months later as odor complaints, curled edges, or yellow stains, and most trace back to the plasticizer package. Our guide on how to choose a plasticizer for a vinyl flooring product starts with the same four challenges.
Indoor Air Quality & FloorScore/AgBB Low-VOC Emission
FloorScore certification follows the CDPH Standard Method for chamber emissions, and Germany’s AgBB scheme caps total VOC at 1.0 mg/m³ and total SVOC at 0.1 mg/m³ after 28 days. Lighter plasticizers and residual ink solvents show up in those results, so the choice of a low VOC plasticizer for PVC flooring often decides pass or fail.
Dimensional Stability & Edge Curling
LVT planks and sheet goods must pass heat dimensional stability and curling tests under EN ISO 23999, run for 6 hours at 80 °C. Plasticizer migrating between layers with different loadings creates uneven shrinkage, and the plank curls or the seam opens after installation.
Stain Resistance & Plastisol Wear-Layer Clarity
Asphalt sealer, hair dye, shoe-heel rubber, and marker ink all stain vinyl by dissolving into the plasticized wear layer. Strong-solvating plasticizers that sit near the surface make staining worse, and poorly matched blends haze the clear wear layer over the print film.
Plastisol Viscosity Control in Multi-Layer Sheet Flooring
Rotary-screen and knife coaters need plastisol that stays inside a narrow viscosity window for days. Plastisol that thickens in the tank causes gauge variation and streaks, while plastisol that runs too thin soaks into the glass-fleece carrier and loses coat weight.
Recommended BASTONE Plasticizers for PVC Flooring
The products below run from the most widely used LVT flooring plasticizer to a specialty viscosity reducer. Most flooring lines combine one primary plasticizer with TXIB or a secondary plasticizer in specific layers.
DOTP (Dioctyl Terephthalate)
LVT & Commercial StandardDOTP for vinyl flooring has become the default primary plasticizer in LVT and commercial heterogeneous sheet. As a terephthalate, it sits outside ortho-phthalate restrictions and gives buyers a phthalate-free product without the cost of a cyclohexane plasticizer.
DOTP has lower volatility than DOP and good permanence in highly filled cores, which helps planks hold their dimensions through heat testing. DOTP plastisols stay stable in the tank but gel slower than DINP, so many lines add TXIB or a fast-fusing secondary to keep oven speed. Bastone DOTP specifies purity ≥ 99.5% and acid value ≤ 0.02 mgKOH/g.
LVT and LVP cores and backings, commercial heterogeneous sheet, homogeneous flooring, and flexible vinyl rolls for retail and healthcare spaces.
DINCH
Ultra-Low VOC / FloorScoreDINCH is the hydrogenated counterpart of DINP: its aromatic ring is saturated into a cyclohexane ring, which removes it from every phthalate list. Bastone DINCH specifies phthalate content of ≤ 0.01 wt% and ester content of ≥ 99.6%, keeping phthalate traces negligible in the finished floor.
Residential, school, and healthcare floors sold against FloorScore, AgBB, or green-building credits often specify DINCH. It delivers low emissions, low migration, and low plastisol viscosity. DINCH solvates PVC more slowly than DINP, so plastisols need a higher fusion temperature or a fast-gelling secondary.
Residential sheet and LVT, school and nursery flooring, healthcare floors, and any product targeting FloorScore, AgBB, or children’s-environment requirements.
DINP (Diisononyl Phthalate)
High-Wear IndustrialDINP gives fast fusion, strong solvating power, and low volatility at a price that suits heavy-gauge flooring. It builds tough, abrasion-resistant compounds for industrial tiles, interlocking garage tiles, and transport floors.
DINP is an ortho-phthalate, and REACH Annex XVII restricts it in toys and childcare articles that children can place in the mouth. For industrial and commercial floors outside those categories, DINP remains a practical primary plasticizer, often blended with DOTP to balance fusion speed and compliance. Bastone DINP specifies flash point ≥ 214 °C and purity ≥ 99.5%.
Industrial and warehouse tiles, interlocking garage and gym tiles, transport flooring, and highly filled compact layers where fusion speed matters.
TXIB
Stain-Resistant & Viscosity ReducerTXIB (2,2,4-trimethyl-1,3-pentanediol diisobutyrate) is a non-phthalate diester with a viscosity of 9 mPa·s at 25 °C. Replacing 5–15 phr of the primary plasticizer with TXIB drops plastisol viscosity sharply, letting coaters run more filler or faster line speeds. In a TXIB flooring plastisol wear layer, it also produces a harder, less tacky surface that resists staining and soil pickup.
TXIB boils at 280–281 °C and has a flash point of 136 °C, so it is more volatile than the other plasticizers on this page. Keep it in the wear layer at modest loadings, and confirm emissions on finished samples before claiming FloorScore or AgBB compliance.
Clear plastisol wear layers, printed sheet flooring, highly filled plastisols that need viscosity reduction, and stain-resistant top layers for vinyl tile.
Comparing Vinyl Flooring Plasticizers
Emissions, fusion speed, and cost rarely line up in the same product. Use the matrix below to set the primary plasticizer, then add TXIB where viscosity or stain resistance needs work.
Current market pricing for all four grades is on our latest plasticizer price page.
| Property | DOTP | DINCH | DINP | TXIB |
|---|---|---|---|---|
| Low VOC / SVOC Emission | ★★★★☆ | ★★★★★ | ★★★★☆ | ★★☆☆☆ |
| Dimensional Stability (Permanence) | ★★★★☆ | ★★★★☆ | ★★★★☆ | ★★☆☆☆ |
| Fusion / Gelation Speed | ★★★☆☆ | ★★☆☆☆ | ★★★★☆ | ★★★☆☆ |
| Plastisol Viscosity Reduction | ★★★☆☆ | ★★★★☆ | ★★★☆☆ | ★★★★★ |
| Wear-Layer Stain Resistance | ★★★☆☆ | ★★★☆☆ | ★★★☆☆ | ★★★★☆ |
| Phthalate-Free | Yes (Terephthalate) | Yes (Cyclohexane) | No (Ortho-Phthalate) | Yes (Diisobutyrate) |
| Typical Flooring Use | LVT Cores, Commercial Sheet | Residential, School, Healthcare | Industrial & Garage Tiles | Wear Layers, Viscosity Control |
Formulation Tips for Vinyl Flooring
Bastone Solution: TXIB at 5–15 phr in Wear Layers
Replace 5–15 phr of DOTP or DINCH in the clear wear-layer plastisol with TXIB to cut viscosity and harden the surface against stains. Start at 8 phr, measure Brookfield viscosity at 1 hour and 24 hours, and run a stain panel with asphalt, mustard, and marker before going higher. Above 15 phr, TXIB adds measurable SVOC emissions and lowers wear-layer permanence.
Bastone Solution: DOTP or DINCH with PR-450 for Cushioned Foam
For chemically foamed cushion layers, pair DOTP or DINCH with a foaming-grade PVC paste resin such as Formolon PR-450 (K-65). Both plasticizers gel slower than DINP, so tune oven temperature or the azodicarbonamide/zinc oxide kicker level until gelation and gas release overlap. Our guide to PVC paste resin grades for flooring, wallpaper, and leather covers resin selection.
Preventing Adhesive Bleed and Edge Curling
Plasticizer migrating from the backing into a glue-down adhesive softens the bond line, which shows up as bleed-through stains and lifted edges. Keep plasticizer loading close between adjacent layers, specify a plasticizer-resistant acrylic adhesive, and favor DINCH or DINP over lighter plasticizers in the backing. Run EN ISO 23999 heat testing on full-construction samples, not single layers.
Bastone Solution: Managing FloorScore and REACH Compliance
Build the compliance file before the first production run. Request a COA and SDS for every plasticizer lot, specify DINCH or DOTP for residential and school floors, and reserve DINP for industrial products outside the REACH Annex XVII toy and childcare categories. Send finished samples for CDPH chamber testing early, since TXIB level and residual ink solvents often decide the result.
Need Help Selecting the Right Plasticizer?
Share your flooring construction, layer thicknesses, target certifications (FloorScore, AgBB, or REACH), and line conditions, and our application engineers will recommend a plasticizer package for each layer.