TXP Trixylenyl Phosphate — Flame-Retardant Plasticizer & Lubricant Additive (CAS 25155-23-1)

Trixylenyl phosphate (TXP) is an organophosphate ester produced by Bastone Plastics, offering a combination of flame retardancy, low volatility, and thermal-oxidative stability in a single compound.

With a flash point of 240°C and an acid value of 0.15 mgKOH/g, TXP serves industrial formulators working in fire-resistant hydraulic fluids, steam turbine lubricants, and PVC plasticizer applications. Bastone supplies TXP factory-direct from its production facilities in Zhejiang, China, with export documentation and flexible packaging for bulk buyers.

CAS No. 25155-23-1

Molecular Formula: C24H27O4P

Other Synonyms: tris(3,5-dimethylphenyl) phosphate

Packaging: 200L drum; IBC

Description

TXP belongs to the aryl phosphate ester family — a class of compounds distinguished from conventional phthalate or adipate plasticizers by their inherent phosphorus-based flame retardancy. The phosphorus content in the molecular structure interrupts combustion cycles, which is why formulators reach for TXP in applications where fire resistance is a regulatory or performance requirement, not just a nice-to-have. The CAS number 25155-23-1 covers the mixed xylenyl isomer product that is commercially standard.

Bastone's TXP carries a flash point of ≥235°C with a typical measured value of 240°C. For lubricant and hydraulic fluid manufacturers, that figure matters considerably: fire-resistant hydraulic fluids used near furnaces, presses, or turbines must survive high-temperature environments without igniting on contact with hot metal surfaces. The flash point of 240°C positions TXP well above most mineral oils and many synthetic alternatives, making it a formulation anchor for anti-combustion fluid development in metallurgy, power generation, and heavy mechanical engineering.

Low acid value is equally important for lubricant applications. TXP's acid value of 0.15 mgKOH/g (specification maximum: 0.5) indicates minimal free acid content, which translates to less corrosive attack on metal surfaces in hydraulic circuits and turbine housings. Combined with TXP's documented thermal-oxidative stability, formulators get a base fluid component that resists breakdown under continuous high-temperature cycling. In steam turbine applications specifically, where the lubricant stays in service for extended periods at elevated temperatures, acid buildup accelerates metal corrosion and sludge formation — a low acid value at the outset reduces that risk.

The specific gravity of 1.132 at 20°C is consistent with aryl phosphate chemistry and relevant to blending calculations. Formulators working with density-sensitive systems (for example, certain hydraulic circuits where fluid density affects pressure transmission characteristics) can use the typical value of 1.132 as a formulation input without relying on estimates.

As a plasticizer in PVC and synthetic rubber systems, TXP adds flame-retardant character to flexible formulations. Wire and cable jacketing, conveyor belting, and industrial hose compounds that need to pass UL or IEC flame-spread tests benefit from TXP as a partial replacement for standard non-FR plasticizers. Bastone supplies TXP from dedicated production infrastructure with batch-level quality documentation, giving downstream compounders a consistent starting point for formulation.

Regulatory note (EU): Trixylyl phosphate (CAS 25155-23-1) is listed in REACH Annex XIV (entry 47, toxic for reproduction) with a sunset date of 27 May 2023. Placing it on the EU market or using it in the EU now requires an authorisation. For flame-retardant flexible PVC sold into the EU, ask us about TCPP or TEP.

Factory and Activities

Specifications

TXP Trixylenyl Phosphate — high-purity aryl phosphate ester
TXP Trixylenyl Phosphate — high-purity aryl phosphate ester, factory-direct from Bastone Plastics.

General Information

Parameter Value
Product Name Trixylenyl Phosphate
Common Abbreviation TXP
CAS Number 25155-23-1
Chemical Family Aryl phosphate ester
Appearance Colorless or light yellow transparent liquid
Export Entity Zhejiang Bastone Technology Co., Ltd

Technical Properties

Parameter Specification Typical Value Unit
Acid Value ≤0.5 0.15 mgKOH/g
Chroma ≤250 200–250 APHA
Specific Gravity (20°C) ≤1.160 1.132 g/cm³
Flash Point ≥235 240 °C

Applications

Fire-Resistant Hydraulic Fluids

Steam turbines and hydraulic systems operating near ignition hazards — foundries, rolling mills, power stations — require fluids that will not sustain combustion if a line ruptures near a hot surface. TXP's flash point of 240°C and inherent phosphate ester flame resistance make it a primary base component or additive in anti-combustion hydraulic oil formulations. The thermal-oxidative stability extends fluid service life under continuous high-temperature operation, reducing the frequency of fluid changes and associated downtime.

Lubricant Additives and Extreme-Pressure Applications

Beyond straight fire resistance, TXP functions as a lubricity additive and anti-wear agent in lubricating oil formulations. Phosphate esters form protective boundary films on metal surfaces under high contact pressure, reducing wear on gears, bearings, and sliding components. The low acid value of 0.15 mgKOH/g means the additive package introduces minimal corrosive species into the finished lubricant, which matters for systems with brass, bronze, or aluminum components that are sensitive to acid attack.

PVC Flame-Retardant Plasticizer

In flexible PVC compounding, TXP functions as a secondary plasticizer paired with primary plasticizers like DINP or DOP. The phosphorus content contributes measurable flame-retardant performance, which is useful for wire and cable insulation, industrial hose, and conveyor belt compounds required to meet fire-spread classifications. Formulators typically use TXP as a partial replacement (10–20 phr range is common in the industry) to achieve FR performance without sacrificing the flexibility provided by primary plasticizers.

Metallurgy, Power, and Mechanical Engineering Fluids

Heavy industrial sectors — steel mills, paper mills, die casting facilities — specify fire-resistant hydraulic fluids where standard mineral oil creates unacceptable fire risk. TXP-based fluids meet this need while delivering the viscosity stability and metal compatibility demanded by high-cycle hydraulic systems. The combination of hydrolysis resistance and oxidative stability keeps fluid properties predictable across operating cycles.

TXP enabling flame-retardant PVC wire and cable jacketing in extrusion manufacturing
TXP enables flame-retardant PVC wire and cable jacketing in high-volume extrusion manufacturing.

Why Choose BASTONE

Bastone Plastics IBC tanks and drums with export documentation
Bastone Plastics supplies TXP in IBC tanks and drums with full export documentation for global buyers.

Bastone Plastics manufactures TXP at its own production facilities in Zhejiang province. Buyers source factory-direct, which eliminates the trading margin built into re-seller pricing and gives procurement teams direct access to production schedules and capacity planning. For industrial fluid formulators and PVC compounders running consistent monthly volumes, that supply chain directness matters during periods of raw material tightness.

Bastone's R&D team works across the full phosphate ester and phthalate plasticizer portfolio, which means technical support on TXP draws from genuine formulation experience — not just a product data sheet forwarded from a source supplier. When a wire and cable customer needs help optimizing a flame-retardant compound for a specific IEC test requirement, Bastone's application engineers can engage at the formulation level, not just the commercial level.

Export logistics from Zhejiang are well-established. Bastone coordinates FCL and LCL shipments, provides standard commercial documentation (COA, TDS, SDS, bill of lading, phytosanitary where required), and works within standard trade terms including FOB, CIF, and CFR. Sample availability for qualification testing is standard practice for new accounts.

Sourcing & Logistics

Parameter Details
Standard Packaging 200 kg net iron drums
Bulk Packaging 1,000 L IBC (upon request)
Export Entity Zhejiang Bastone Technology Co., Ltd
Documentation COA, TDS, SDS, Bill of Lading
Trade Terms FOB, CIF, CFR (negotiable)
Sample Availability Available for qualified buyers
Storage Requirements Store in cool, dry conditions away from heat sources

TEP Triethyl Phosphate (CAS 78-40-0) — Flame Retardant Plasticizer for PVC and CoatingsTEP Triethyl Phosphate (CAS 78-40-0) — Flame Retardant Plasticizer for PVC and Coatings
Bastone's TEP (triethyl phosphate) is a high-purity organophosphate…
TCPP (Tris(1-Chloro-2-Propyl) Phosphate) | Flame Retardant Plasticizer — CAS 13674-84-5TCPP (Tris(1-Chloro-2-Propyl) Phosphate) | Flame Retardant Plasticizer — CAS 13674-84-5
Bastone STONEAF-TCPP is a chlorinated organophosphate flame retardant…
TCEP Tris(2-Chloroethyl) Phosphate — Flame Retardant Plasticizer (CAS 115-96-8)TCEP Tris(2-Chloroethyl) Phosphate — Flame Retardant Plasticizer (CAS 115-96-8)
Bastone supplies TCEP (Tris(2-chloroethyl) phosphate, CAS 115-96-8) as…

Online Message

If you have any questions, you can leave a message here, we will contact you within 24 hours

Contact us

Get quote for your products or ask for a unique solution . We are here to provide quality products and flexible service.