Plasticizer DOP (Dioctyl phthalate)
CAS No. 117-81-7
Molecular Formula: C24H38O4
Other Synonyms: DOP Oil
Application: General purpose plasticizer for PVC
Packaging: IBC, DRUM, Flexi bag
BASTONE is the leading DOP manufacturer and supplier in China, with years of experience as a reliable producer and exporter of plasticizers.
Description
Plasticizer DOP is one of the most effective plasticizers in terms of plasticizing performance, while also being cost-effective. Therefore, DOP (Dioctyl Phthalate) is the most used plasticizer. BASTONE is the leading DOP manufacturer and supplier in China, with years of experience as a reliable producer and exporter of plasticizers.
DOP is widely used in PVC film, cables(insulation grade), conveyor belt, transparent hose, ordinary artificial leather, enamel toys, packing material, PVC gloves and wallpapers etc. As a high-performance plasticizer, it significantly improves the flexibility, durability, and workability of PVC materials.
Our facility uses advanced technologies and strict quality control to ensure consistent performance in your applications. We provide DOP with excellent compatibility with PVC resins, making it an ideal choice for various soft PVC products.
BASTONE Plasticizers Enhance the performance of your PVC products. The leading DOP producer (manufacturer) in China
Specifications
Appearance | Transparent oily liquid |
---|---|
Chroma | ≤30 |
Purity | ≥99.5% |
Density(20℃) | 0.982-0.988 g/cm3 |
Flash Point | ≥196℃ |
Acidity | ≤0.030% |
Water | ≤0.10% |
Online Message
If you have any questions, you can leave a message here, we will contact you within 24 hours
Contact us
Get quote for your products or ask for solution for the compounds which you can’t find in the market. We are here to provide flexible service and contract manufacturing compound for you.