Plasticizer Price Daily|June 26, 2025|DOP producer

Brief analysis:

DOP,DOTP price is adjusted by -USD6/TON, DINP price -USD15/TON

BASTONE suggestion:

expect price increase after summer, good time to buy at current price level

Important information: it is reference price for public. For actual inquiry/demand, please conact us via submitting message in Contact Form.